Polystyrène - Bloc - poly (éthylène - ran-butylène)-Bloc-polystyrène - implant - anhydride maléique, indice de fonte environ 21 g/10 min. (230 C / 5,0 kg)

Code: 432431-250g D2-231

Non disponible en dehors du Royaume-Uni et de l'Irlande

Application

Component of hot melt adhesives, sealants, asphalt and oil gels. Modifier for polymers, thermosets and general rubber compounding. Direct molded or extruded auto ...


en savoir plus

Votre prix
$58.19 250G

Non disponible en dehors du Royaume-Uni et de l'Irlande

Application

Component of hot melt adhesives, sealants, asphalt and oil gels. Modifier for polymers, thermosets and general rubber compounding. Direct molded or extruded auto parts, sporting goods, footware and film.

Features and Benefits

Maleic anhydride is grafted on the mid-block to increase compatibility with polar coatings and increase interaction with substrates. More oxidatively stable than unsaturated precursor. Flexible to -80°C.

Packaging

250 g in poly bottle

Physical form

Thermoplastic elastomer.

compositionmaleic anhydride, ~2 wt. %
density0.91 g/mL at 25 °C (lit.)
elongationASTM D 412 - 500% (ultimate)
formpellets
hardness75 (Shore A)
melt index~21 g/10 min (230°C/5.0kg)
Quality Level200
SMILES stringC=C.C=CC=C.O=C1OC(=O)C=C1.C=Cc2ccccc2
solubilitysolvents with solubility parameters between 7.7 and 9.4: soluble
viscosity12.5 poise, 15 wt. % in toluene(25 °C, Brookfield)(lit.)
Cas Number124578-11-6