Graphene preparation method: Electrochemical exfoliation. Graphene thickness by AFM: 80%, 1-3 layers. Sheet size by AFM: 10 µm. Oxygen content: 7.5% (by XPS) (C/O-ratio: 12.3). Raman I_D/I_G ratio: 0.4. Sheet resistance: 4.8 kΩ/sq. Typical properties of films produced thereof (after spray coating): a) 11 nm film: 90% transmittance, 1200 Ω/sq (as made). b) 20 nm film: 80% transmittance, 500 Ω/sq (as made).
Packaging
50 mL in glass bottle